Preparation and Mechanism Study of Reversible Thermochromic Materials for Monitoring Abnormal Heating in Composite Insulators
Hu Qin1, Du Jiaoyang1, Jiang Zeshen2, Wang Huan1, Jiang Xingliang1
1. State Key Laboratory of Power Transmission Equipment Technology Chongqing University Chongqing 400044 China; 2. Shibei Power Supply Branch State Grid Chongqing Electric Power Company Chongqing 401120 China
Abstract:Abnormal heating in composite insulators poses a serious threat to the safe and stable operation of transmission lines, necessitating temperature monitoring and identification. However, existing temperature measurement methods suffer from issues such as significant accuracy fluctuations due to environmental factors, high costs, and poor localization capabilities. Furthermore, as voltage-induced heating devices, composite insulators lack clear thermal failure temperature thresholds. To address these challenges, this paper presents a novel reversible thermochromic material specifically developed for this purpose. This material enables transitions between multiple stable color states. First, extensive research was conducted on thermal failure cases of composite insulators. By analyzing ambient temperatures and surface temperatures of failed insulators, the color-changing temperature range for the material was determined. Based on the color wheel theory, the material's color manifestation was defined. Second, the thermochromic material was prepared using a three-component method (thermochromic dye, developer, and solvent). The thermochromic performance of materials with different ratios was compared, and the optimal formulation for the corresponding temperature range was selected. Finally, Fourier transform infrared spectroscopy (FTIR) and differential scanning calorimetry (DSC) tests were conducted on the prepared thermochromic material and various composites to analyze the cause of color change and the response mechanism to temperature variations. Considering both accident frequency and potential risks, the color-changing temperature ranges were selected as 33~37℃ and 43~47℃. For the color-revealing states, blue and green were chosen to create a strong visual contrast with the brick-red housing. Based on these criteria, this study developed a novel reversible thermochromic material featuring two thermochromic systems capable of three steady-state color transitions: System 1 employs a conventional colored-to-colorless (upon heating) phase change, while System 2 utilizes an innovatively developed colorless-to-colored (upon heating) phase change. The optimal formulations are crystal violet lactone: bisphenol A: 1-tetradecanol (1:8:130) and thermochromic green: dodecyl gallate: 1-tetradecanol (1:7:90), respectively. FTIR indicates that thermochromic green color change the opening of the lactone ring and strong interactions with the developer. At room temperature, System 2 remains colorless because the developer exhibits stronger interactions with the solvent than with the thermochromic dye, and the developer-solvent composite shares highly similar spectral characteristics with the thermochromic material. DSC analysis indicates that the presence of the developer disrupts the crystal lattice integrity of 1-tetradecanol, interfering with the phase transition process. This leads to an elevated color change temperature and a slowed color change rate for the material. Through data comparison and analysis, the following conclusions can be drawn: (1) Heating incidents in composite insulators exhibit a strong correlation with ambient temperature. (2) The novel thermochromic material developed in this study rapidly changes color upon heating and slowly reverts upon cooling, effectively capturing and recording heating faults in composite insulators. (3) The type of developer influences the thermochromic dynamics and the formation of new systems. (4) The cause of material color change is the opening of the lactone ring in the thermochromic dye and the resulting expansion of the conjugated system. The conditions for material color change are changes in the strength of interactions among the three components. The formation of a new colorless-to-colored (upon heating) system occurs because the interaction forces between the developer and solvent at room temperature are stronger than those with the thermochromic dye.
胡琴, 杜娇杨, 江泽申, 王欢, 蒋兴良. 复合绝缘子异常发热监测用可逆示温变色材料制备及其机理研究[J]. 电工技术学报, 2026, 41(21): 7213-7225.
Hu Qin, Du Jiaoyang, Jiang Zeshen, Wang Huan, Jiang Xingliang. Preparation and Mechanism Study of Reversible Thermochromic Materials for Monitoring Abnormal Heating in Composite Insulators. Transactions of China Electrotechnical Society, 2026, 41(21): 7213-7225.
[1] 梁曦东, 仵超, 左周, 等. 高电压有机外绝缘发展综述与展望[J]. 中国电机工程学报, 2024, 44(18): 7412-7425, I0024. Liang Xidong, Wu Chao, Zuo Zhou, et al.Review and prospects for development of high voltage outdoor organic insulation[J]. Proceedings of the CSEE, 2024, 44(18): 7412-7425, I0024. [2] 谢从珍, 李煜, 苟彬, 等. 湿热环境下含芯棒-护套界面缺陷复合绝缘子的界面老化机制研究[J]. 绝缘材料, 2024, 57(4): 72-81. Xie Congzhen, Li Yu, Gou Bin, et al.Study on interface ageing mechanisms of composite insulators with core-sheath interface defects under hygrothermal environment[J]. Insulating Materials, 2024, 57(4): 72-81. [3] 胡琴, 陈旭烨, 闻君, 等. 强暴雨天气下复合悬式绝缘子交流闪络特性[J]. 电工技术学报, 2025, 40(9): 2970-2981. Hu Qin, Chen Xuye, Wen Jun, et al.AC flashover characteristics of composite suspension insulators under heavy rainstorm[J]. Transactions of China Electrotechnical Society, 2025, 40(9): 2970-2981. [4] 覃永雄, 虞澜, 傅佳, 等. 长波紫外照射下高温硫化硅橡胶的微观物性及憎水性研究[J]. 电工技术学报, 2014, 29(12): 242-250. Qin Yongxiong, Yu Lan, Fu Jia, et al.Research on microscopic properties and hydrophobicity of high temperature vulcanization silicone rubber under long-wave ultraviolet radiation[J]. Transactions of China Electrotechnical Society, 2014, 29(12): 242-250. [5] 曹雯, 杨特, 申巍, 等. 变湿度条件下不同老化程度复合绝缘子的红外温升行为及特征分析[J]. 电工技术学报, 2025, 40(17): 5601-5614. Cao Wen, Yang Te, Shen Wei, et al.Infrared temperature rise behavior and characteristic analysis of composite insulators with different aging degrees under variable humidity conditions[J]. Transactions of China Electrotechnical Society, 2025, 40(17): 5601-5614. [6] 张志劲, 张翼, 蒋兴良, 等. 自然环境不同年限复合绝缘子硅橡胶材料老化特性表征方法研究[J]. 电工技术学报, 2020, 35(6): 1368-1376. Zhang Zhijin, Zhang Yi, Jiang Xingliang, et al.Study on aging characterization methods of composite insulators aging in natural environment for different years[J]. Transactions of China Electrotechnical Society, 2020, 35(6): 1368-1376. [7] 张血琴, 周志鹏, 郭裕钧, 等. 不同材质绝缘子污秽等级高光谱检测方法研究[J]. 电工技术学报, 2023, 38(7): 1946-1955. Zhang Xueqin, Zhou Zhipeng, Guo Yujun, et al.Detection method of contamination grades of insulators with different materials based on hyperspectral technique[J]. Transactions of China Electrotechnical Society, 2023, 38(7): 1946-1955. [8] 范建斌, 殷禹, 张锦秀, 等. 复合绝缘子运行状况评估方法[J]. 电网技术, 2006, 30(12): 24-28. Fan Jianbin, Yin Yu, Zhang Jinxiu, et al.Evaluation methods for operational status of composite insulators[J]. Power System Technology, 2006, 30(12): 24-28. [9] 沈瑶, 刘兴杰, 梁英, 等. 基于硅橡胶分子链陷阱变化的复合绝缘子老化现象[J]. 电工技术学报, 2024, 39(17): 5545-5554. Shen Yao, Liu Xingjie, Liang Ying, et al.Aging phenomenon of composite insulators based on chemical traps’ change of silicone rubber molecular chain[J]. Transactions of China Electrotechnical Society, 2024, 39(17): 5545-5554. [10] 刘康, 李彦茹, 王津, 等. 强风环境中330 kV Ⅰ串硅橡胶复合绝缘子伞裙形变特性及抗偏折结构设计[J]. 绝缘材料, 2025, 58(9): 118-128. Liu Kang, Li Yanru, Wang Jin, et al.Deformation characteristics and anti-deflection structural design of umbrella skirt for 330 kV Ⅰ-string silicone rubber composite insulators in strong wind environment[J]. Insulating Materials, 2025, 58(9): 118-128. [11] 梁曦东, 高岩峰. 复合绝缘子酥朽断裂研究(一): 酥朽断裂的主要特征、定义及判据[J]. 中国电机工程学报, 2016, 36(17): 4778-4785. Liang Xidong, Gao Yanfeng.Study on decay-like fracture of composite insulator: part Ⅰ- the principal character, definition and criterion of decay-like fracture[J]. Proceedings of the CSEE, 2016, 36(17): 4778-4785. [12] 高岩峰, 梁曦东. 复合绝缘子酥朽断裂研究(二): 酥朽断裂的试验模拟及预防措施讨论[J]. 中国电机工程学报, 2016, 36(18): 5070-5077, 5132. Gao Yanfeng, Liang Xidong.Study on decay-like fracture of composite insulator, part Ⅱ: experimental simulation and preventive method discussion of decay-like fracture[J]. Proceedings of the CSEE, 2016, 36(18): 5070-5077, 5132. [13] 周靖翔, 徐祖顺. 新型三重示温涂层材料的制备及其性能研究[J]. 胶体与聚合物, 2022, 40(4): 159-161. Zhou Jingxiang, Xu Zushun.Preparation and properties of novel triple temperature-indicating coating materials[J]. Chinese Journal of Colloid & Polymer, 2022, 40(4): 159-161. [14] 高燕, 刘晓艳, 郝鸿飞, 等. 十四醇-十六醇二元体系热致变色材料的研制[J]. 纺织学报, 2016, 37(1): 70-74. Gao Yan, Liu Xiaoyan, Hao Hongfei, et al.Preparation of tetradecanol-hexadecanol binary mixture thermochromic materials[J]. Journal of Textile Research, 2016, 37(1): 70-74. [15] 贾贞, 贾东哲, 包文慧. 可逆温敏变色聚氨酯水泥复合材料制备及其响应行为研究[J]. 功能材料, 2022, 53(6): 6159-6163. Jia Zhen, Jia Dongzhe, Bao Wenhui.Preparation and response behavior of reversible thermochromic polyurethane cement composites[J]. Journal of Functional Materials, 2022, 53(6): 6159-6163. [16] 宋晓丽, 李字明, 陈靖文, 等. 热致变色材料在智能社会中的发展现状及趋势[J]. 精细化工, 2020, 37(3): 452-461. Song Xiaoli, Li Ziming, Chen Jingwen, et al.Smart applications of thermochromic materials for intelligent society: Latest development and future perspective[J]. Fine Chemicals, 2020, 37(3): 452-461. [17] 谷山强, 王海涛, 严碧武, 等. 基于示温涂料的输电线路金具发热故障诊断[J]. 水电能源科学, 2017, 35(11): 186-189. Gu Shanqiang, Wang Haitao, Yan Biwu, et al.Heating fault diagnosis for hardware of power transmission line based on temperature sensitive paints[J]. Water Resources and Power, 2017, 35(11): 186-189. [18] 黄洪松. 三芳甲烷类电气设备发热故障示温材料制备与性能研究[D]. 重庆: 重庆大学, 2021. Huang Hongsong.Study on the preparation and performance of triarylmethane temperature indicating material for electrical equipment[D]. Chongqing: Chongqing University, 2021. [19] 董冰冰, 孟岩, 葛医博, 等. 隔离开关温度检测用可逆变色涂料制备方法及其性能[J]. 高电压技术, 2024, 50(6): 2580-2589. Dong Bingbing, Meng Yan, Ge Yibo, et al.Preparation method of reversible color-changing coating for temperature detection of disconnect switches and its performance[J]. High Voltage Engineering, 2024, 50(6): 2580-2589. [20] 董冰冰, 武奔, 孟岩. 用于干式空心电抗器热致缺陷的可逆示温涂料制备与变色理化特性[J]. 高电压技术, 2024, 50(1): 322-330. Dong Bingbing, Wu Ben, Meng Yan.Preparation of reversible thermochromic coatings for dry hollow reactors with thermal defects and the physicochemical properties of discoloration[J]. High Voltage Engineering, 2024, 50(1): 322-330. [21] 王雅群, 陈萌, 周桂月, 等. 电力设备测温用可逆热致变色材料的老化特性研究[J]. 绝缘材料, 2018, 51(12): 16-22. Wang Yaqun, Chen Meng, Zhou Guiyue, et al.Ageing characteristics of reversible thermochromic materials used for temperature measurement of power equipment[J]. Insulating Materials, 2018, 51(12): 16-22. [22] DL/T 664—2016 带电设备红外诊断应用规范[S]. [23] 卢明, 高超, 李子岳, 等. 复合绝缘子酥朽断裂事故的分布规律研究[J]. 高压电器, 2024, 60(2): 133-142. Lu Ming, Gao Chao, Li Ziyue, et al.Study on distribution of decay-like fracture of composite insulator[J]. High Voltage Apparatus, 2024, 60(2): 133-142. [24] 王信刚, 雷为愉, 朱街禄, 等. 可逆热致变色相变微胶囊的热响应及光热转换性能[J]. 材料导报, 2023, 37(20): 194-199. Wang Xingang, Lei Weiyu, Zhu Jielu, et al.Thermal response and photothermal conversion performance of reversible thermochromic phase change microcapsules[J]. Materials Reports, 2023, 37(20): 194-199. [25] 王鹏, 张雪松, 陈涛, 等. 超疏水可逆热致变色智能感温涂层的制备及其性能的研究[J]. 中国电机工程学报, 2023, 43(9): 3642-3650. Wang Peng, Zhang Xuesong, Chen Tao, et al.Study on preparation and performance of superhydrophobic reversible thermochromic intelligent temperature sensitive coating[J]. Proceedings of the CSEE, 2023, 43(9): 3642-3650. [26] 张凤, 管萍, 胡小玲. 有机可逆热致变色材料的变色机理及应用进展[J]. 材料导报, 2012, 26(9): 76-80. Zhang Feng, Guan Ping, Hu Xiaoling.Color-changing mechanism and application development of organic reversible thermochromic materials[J]. Materials Review, 2012, 26(9): 76-80.