Abstract:In order to study on the aging characteristic of silicone rubber sheds of 110kV composite insulators, 9 silicone rubber composite insulators running in 3 different regions with 110kV were study with the Fourier transform infrared spectrum(FTIR) method. The FTIR difference of the silicon rubber sheds running with different electric field level, service environment and operating years were analyzed. The results indicate that the FTIR of the rubber silicon shed with higher electric field, more serious pollution environment and longer running years is smaller. At the same time, it is shown that the rubber silicon shed with higher electric field, more serious pollution environment and longer running years also aged more seriously. Moreover, the aging velocity of the rubber silicon shed increased slowly in the first 9 years running time, then increased sharply and become slowly after 13years running time. The operating year deteriorates the silicon rubber sheds more seriously than electric field and service environment. The SEM photographs of the silicon rubber sheds were also analyzed to demonstrate the surface deterioration of silicon rubber sheds.
汪佛池, 律方成, 杨升杰, 刘杰, 李宁彩. 基于FTIR的110kV复合绝缘子硅橡胶伞裙老化性能分析[J]. 电工技术学报, 2015, 30(8): 297-303.
Wang Fochi, Lü Fangcheng, Yang Shengjie, Liu Jie, Li Ningcai. The Aging Characteristic of Silicon Rubber Sheds of 110kV Composite Insulators Based on FTIR Test. Transactions of China Electrotechnical Society, 2015, 30(8): 297-303.
[1] 刘泽洪. 复合绝缘子使用现状及其在特高压输电线路中的应用前景[J]. 电网技术, 2006, 30(12): l-7. Liu Zehong. Present situation and prospects of applying composite insulators to uhf transmission lines in china [J]. Power System Technology, 2006, 30(12): l-7. [2] Mackevich J, Shah M. Polymer outdoor insulating materials. Part I: comparison of porcelain and polymer electrical insulation[J]. IEEE Transactions on Electrical Insulation Magazine, 1997, 13(3): 5-12. [3] 关志成. 绝缘子及输变电设备外绝[M]. 北京: 清华大学出版社, 2006. [4] 宿志一, 陈刚, 李庆峰, 等. 硅橡胶复合绝缘子伞裙护套的老化及其判据研究[J]. 电网技术, 2006, 30(12): 53-57. Su Zhiyi, Chen Gang, Li Qingfeng, et al. Study on aging and criterion of sheds and housing of silicon rubber composite insulator[J]. Power System Tech- nology, 2006, 30(12): 53-57. [5] 赵林杰. 硅橡胶复合绝缘子憎水性与污闪特性研究[D]. 北京: 华北电力大学, 2008. [6] Rowland S, Robertson J, Xiong Y, et al. Electrical and material characterization of field-aged 400kV silicone rubber composite insulators[J]. IEEE Transac- tions on Dielectrics and Electrical Insulation, 2010, 17(2): 375-383. [7] 屠幼萍, 陈聪慧, 佟宇梁, 等. 现场运行复合绝缘子伞裙材料的老化判断方法[J]. 高电压技术, 2012, 38(10): 2522-2527. Tu Youping, Chen Qionghui, Tong Yuliang, et al. Aging characteristics of shed materials of silicone rubber composite insulators in service[J]. High Voltage Engineering, 2012, 38(10): 2522-2527. [8] Chughtai AR, Smith DM, Kumosa LS, et al. FTIR analysis of non-ceramic composite insulators[J]. IEEE Transactions on Dielections and Electrical Insulation, 2004, 11(4): 585-596. [9] 蓝磊, 文习山, 刘辉. 用红外光谱研究室温硫化硅橡胶电晕老化及寿命估计[J]. 高电压技术, 2009, 35(11): 2652-2656. Lan Lei, Wen Xishan, Liu Hui. Corona aging tests and lifetime evaluation of RTV silicone rubber through FTIR[J]. High Voltage Engineering, 2009, 35(11): 2652-2656. [10] 巫松桢, 谢大荣, 陈寿田, 等. 电气绝缘材料科学与工程[M]. 西安: 西安交通大学出版社, 1996. [11] Seog Hyeon Kim, Cherney E A, Hackam R, et al. Chemical changes at the surface of RTV silicone rubber coatings on insulators during dry-band arcing [J]. IEEE Transactions on Dielectrics and Electrical Insulation, 1994, 1(1): 106-123. [12] Efimenko K, Wallace W E, Genzer J. Surface modifica- tion of Sylgard-184 poly(dimethyl siloxane) networks by ultraviolet andultraviolet/ozone treatment[J]. Journal of Colloid and Interface Science, 2002, 254: 306-315. [13] Moreno V M, Gourur R S. Effect of long-term corona on non-ceramic outdoor insulator housing materials[J]. IEEE Transactions on Dielectrics and Electrical Insulation, 2001, 8(1): 117-128. [14] 蓝磊, 王汉良, 文习山, 等. 高温硫化硅橡胶加速电晕老化试验分析及其寿命预测[J]. 高电压技术, 2012, 38(4): 82-89. Lan Lei, Wang Hanliang, Wen Xishan, et al. Accele- rated corona aging tests analysis and lifetime prediction of HTV silicon rubber[J]. High Voltage Engineering, 2012, 38(4): 82-89. [15] 傅佳, 覃永雄, 王勇, 等. 248nm紫外激光照射高温硫化硅橡胶实验及老化机理探讨[J]. 电网技术, 2012, 36(11): 77-82. Fu Jia, Qin Yongxiong, Wang yong, et al. 248nm ultraviolet laser radiation experiment of high tem- perature vulcanized silicone rubber and its accelerated ageing mechanism[J]. Power System Technology, 2012, 36(11): 77-82. [16] 王建国, 刘洋, 方春华, 等. 交流电晕对高温硫化硅橡胶性能的影响[J]. 高分子学报, 2009, 4: 31-37. Wang Jianguo, Liu Yang, Fang Chunhua, et al. Per- formance influence of high temperature vulcanization silicone rubber by alternating current corona discharge [J]. Acta Polymerica Sinica, 2009, 4: 31-37. [17] 高海峰, 贾志东, 关志成. 运行多年RTV涂料绝缘子表面涂层老化分析研究[J]. 中国电机工程学报, 2005, 25(9): 58-63. Gao Haifeng, Jia Zhidong, Guan Zhicheng. Aging study on RTV coating covered on insulators and energized for many years[J]. Proceedings of the CSEE, 2005, 25(9): 58-63. [18] Moreno V M, Gorur R S, Kroese A. Impact of corona on the long-term performance of nonceramic insulators [J], IEEE Transactions on Dielectrics and Electrical Insulation, 2003, 10(1): 80-95. [19] Xiong Y, Rowland S M, Robertson J, et al. Surface analysis of asymmetrically aged 400kV silicone rubber composite insulators[J]. IEEE Transactions on Dielec- trics and Electrical Insulation, 2008, 15(3): 763-770. [20] 梁曦东, 李震宇, 周远翔. 交流电晕对硅橡胶材料憎水性的影响[J]. 中国电机工程学报, 2007, 27(27): 19-23. Liang Xidong, Li Zhenyu, Zhou Yuanxiang. Influences of AC corona on hydrophobicity of silicone rubber[J]. Proceedings of the CSEE, 2007, 27(27): 19-23.